ASTM A 336 Grade F22V Structural and constructional steels
Data updates
This material has 113 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 336 Grade F22V Chemical Composition
A336/A336M: 2023 / Standard Specification for Alloy Steel Forgings for Pressure and High-Temperature Parts
Looking for full material performance data?
Free registration required • Instant access
ASTM A 336 Grade F22V Physical Properties
Temperature
This material has 113 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 336 Grade F22V Heat Treatments
- The minimum austenitizing temperature shall be 900°C (1650°F).The minimum tempering temperature shall be 675°C (1250°F).
ASTM A 336 Grade F22V Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 336 Grade F22V International Equivalent Materials
Showing 15 of 69 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 69 international equivalents?
See all 69 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 69Cross References
- 14Composition
- 7Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 2Joints
- -Coatings
- 15Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 2Total Suppliers