ISO C37H Cast steels
Data updates
This material has 55 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ISO C37H Chemical Composition
ISO 4991: 1994 / Steel castings for pressure purposes
Looking for full material performance data?
Free registration required • Instant access
ISO C37H Heat Treatments
- Normalized and tempered (N+T): Austenitized at 930-990°C, air cooled. Tempered at 620-750°C, air or furnace cooled
ISO C37H Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ISO C37H International Equivalent Materials
Showing 2 of 42 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 42 international equivalents?
See all 42 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 42Cross References
- 7Composition
- 5Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers