ISO C34BL Cast steels
Data updates
This material has 22 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ISO C34BL Chemical Composition
ISO 4991: 1994 / Steel castings for pressure purposes
Looking for full material performance data?
Free registration required • Instant access
ISO C34BL Heat Treatments
- Normalized and tempered (N+T): Austenitized at 930-970°C, air cooled. Tempered at 680-750°C, air or furnace cooled
Normalized and tempered (Nac+T): Austenitized at 930-970°C, accelerated air cooled. Tempered at 680-750°C, air or furnace cooled
Quenched and tempered (Q+T): Austenitized at 930-970°C, liquid quenched. Tempered at 680-750°C, air or furnace cooled
ISO C34BL Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ISO C34BL International Equivalent Materials
Showing 2 of 10 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 10 international equivalents?
See all 10 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 10Cross References
- 7Composition
- 4Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers