1.5682 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2022-01
Total number of updates: 3
Update History:
2016-05 2014-05

Mechanical Properties


Temperature

≤ 0°C
0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 510 MPa view details
Tensile Strength 690 — 840 MPa view details
Elongation, A 18 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 74 ksi view details
Tensile Strength 100.1 — 121.8 ksi view details
Elongation, A 18 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.13
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
0.30 – 0.80
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2

EN 10216-4: 2013 / Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 4: Non-alloy and alloy steel tubes with specified low temperature properties

Heat Treatments

  • Normalized (+N) at 880-915°C or Normalized at 775-805°C and Tempered at 565-605°C(+N+NT); Quenched and Tempered (QT): Normalizing at 880-930°C, Hardening at 770-820°C, Cooling medium: water or oil, Tempering at 540-600°C.
  • Quenched and tempered (QT):<br>Austenitizing at 770-820°C, water or oil quenched<br>Tempered at 540-660°C, air cooled