1.0725 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2024-12
Total number of updates: 3
Update History:
2018-08 2017-07

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 420 — 840 MPa view details
Elongation, A 6 % view details
Brinell Hardness (HB) 125 — 178 view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 60.9 — 121.8 ksi view details
Elongation, A 6 % view details
Brinell Hardness (HB) 125 — 178 view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.12 – 0.18
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.90 – 1.30
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Other
VALUE
Elements such as Te, Bi etc., may only be added by the manufacturer for improving machinability
UNIT
%
CAS NUMBER
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN 10087: 1998 / Free-cutting steels - Technical delivery conditions for semi-finished products, hot-rolled bars and rods

Heat Treatments

  • Carburizing: 880-980°C. The carburizing temperature will depend on the chemical composition of the steel, the mass of the product, and the carburizing medium. If the steels are direct hardened, in general, a temperature of 950°C is not exceeded. For special procedures, for example under vacuum, higher temperatures (for example 1 020 to 1 050°C) are not unusual; <br /> Core-hardening: 880-920°C. When applying the single quench method, the steel is to be quenched from the carburizing temperature or a lower temperature. The lower hardening temperatures are in each case to be preferred, in particular when there is risk of distortion; Case-hardening: 780-820°C;<br /> Quenching agent: water, oil, emulsion. The kind of quenching agent depends on, for example, the shape of the products, the cooling conditions and the amount of furnace filling;<br /> Tempering: 150-200°C (1 h minimum).