CSN 1.1163 Structural and constructional steels
Data updates
This material has 9231 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
CSN 1.1163 Chemical Composition
EN 10083-1: 1991 / Quenched and tempered steels - Part 1: Technical delivery conditions for special steels (includes amendment A1:1996)
Looking for full material performance data?
Free registration required • Instant access
CSN 1.1163 Physical Properties
Temperature
This material has 9231 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
CSN 1.1163 Heat Treatments
- Austenitizing (quenching in water): 860-900°C, t > 30 min. Tempering: 550-660°C, t > 60 min. Normalizing: 880-920°C, t > 30 min.
CSN 1.1163 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
CSN 1.1163 International Equivalent Materials
Showing 15 of 316 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 316 international equivalents?
See all 316 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 316Cross References
- 29Composition
- 71Mechanical Properties
- 3Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 10Fatigue
- -Fracture
- -Creep
- 83Joints
- -Coatings
- 6Dimensions
- 1Tribology
- 8491Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 219Total Suppliers