Lloyds LR AH 36 Structural and constructional steels
Data updates
This material has 8816 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
Lloyds LR AH 36 Chemical Composition
Rules for the Manufacture, Testing and Certification of Materials, Chapter 3 Section 3; Rolled Steel Plates, Strip, Sections and Bars; Higher strength steels for ship and other structural applications, Lloyd's Register, 2025
Looking for full material performance data?
Free registration required • Instant access
Lloyds LR AH 36 Physical Properties
Temperature
This material has 8816 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
Lloyds LR AH 36 Heat Treatments
- For plates and wide flats, grain refining practice Al or Al+Ti:
t ≤ 20 mm, as-rolled (AR), furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM);
20 < t ≤ 150 mm, furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM) (Material up to 35 mm thick may be supplied in the as-rolled condition provided that prior approval has been obtained from LR);
For plates and wide flats, grain refining practice Nb or V or Al+(Nb or V) or Al+(Ti)+(Nb or V):
t ≤ 12.5 mm, as-rolled (AR), furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM);
12.5 < t ≤ 150 mm, furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM);
For sections and bars, grain refining practice Al or Al+Ti:
t ≤ 20 mm, as-rolled (AR), quench and tempered (QT), furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM);
20 < t ≤ 50 mm, furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM) (Subject to the special approval of LR, sections may be supplied in the as-rolled condition provided satisfactory results are consistently obtained from CharpyV-notch impact tests);
For sections and bars, grain refining practice Nb or V or Al+Nb or Al+V or Al+(Ti)+(Nb or V):
t ≤ 12.5 mm, as-rolled (AR), quench and tempered (QT), furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM);
12.5 < t ≤ 50 mm, furnace normalized (N), normalizing rolled (NR) and thermomechanically controlled rolling (TM) (Subject to the special approval of LR, sections may be supplied in the as-rolled condition provided satisfactory results are consistently obtained from CharpyV-notch impact tests)
Lloyds LR AH 36 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Lloyds LR AH 36 International Equivalent Materials
Showing 15 of 180 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 180 international equivalents?
See all 180 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 180Cross References
- 15Composition
- 26Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 83Joints
- -Coatings
- -Dimensions
- 1Tribology
- 8491Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 16Total Suppliers