IS TP 317 Stainless steels
Data updates
This material has 254 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
IS TP 317 Chemical Composition
IS 11714-5: 1986 / Specification for steel tubes for steel exchangers. Part 5: Electric resistance welded alloy steel tubes
Looking for full material performance data?
Free registration required • Instant access
IS TP 317 Physical Properties
Temperature
This material has 254 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
IS TP 317 Heat Treatments
- The heat treatment procedure, shall consist of heating the material to a minimum temperature of 1040°C and quenching in water or rapidly cooling by other means.
IS TP 317 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
IS TP 317 International Equivalent Materials
Showing 4 of 94 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 94 international equivalents?
See all 94 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 94Cross References
- 8Composition
- 4Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- 144Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers