CNS 631 Stainless steels

Material group: Ferrous Alloys / Stainless steels
Country / Standard: China / CNS

Data updates

Latest Update: 2021-01
Total number of updates: 1
Update History

This material has 72 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CNS 631 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
0.75 – 1.50
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
C
VALUE
≤ 0.09
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
16.00 – 18.00
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

G3067: 1987 / Stainless steel bars

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CNS 631 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 215 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.61 — 8.1 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 72 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CNS 631 Heat Treatments


  • Solutionizing: 1000 - 1100°C, rapid cooling. Precipitation hardening: TH1050: After solutionizing, 760°C +/- 15°C (90 minutes), cool down to 15°C or lower within 1 hour (30 minutes), 565°C +/- 10°C (90 minutes), then air cool. RH950: After solutionizing, 955°C +/- 10°C (10 minutes), air cool down to room temperature, -73°C +/- 6°C within 24 hours (8 hours), 510°C +/- 10°C (60 minutes), then air cool.

CNS 631 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≥ 1030 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
≥ 229
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
≥ 4 %
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 45Cross References

  • 8Composition
  • 14Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers