IS C15Mn75 Structural and constructional steels
Data updates
This material has 291 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
IS C15Mn75 Chemical Composition
IS 6967: 1973 / Steel for electrically welded round link chains
Looking for full material performance data?
Free registration required • Instant access
IS C15Mn75 Physical Properties
Temperature
This material has 291 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
IS C15Mn75 Heat Treatments
- Annealed: 880-950°C; Subcritical annealed: 630-700°C; Normalized: 880-950°C; Carburized: 880-950°C; Refined after carburized: 880-950°C; Hardened: 900-950°C; Hardened after carburized: 760-780°C; Tempered: max. 650°C; Forging/rolling temperature:1250°C;
IS C15Mn75 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
IS C15Mn75 International Equivalent Materials
Showing 15 of 118 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 118 international equivalents?
See all 118 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 118Cross References
- 45Composition
- 52Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 12Creep
- -Joints
- -Coatings
- 26Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 34Total Suppliers