IS X04Cr18Ni10 Stainless steels
Material group:
Ferrous Alloys / Stainless steels
Country / Standard:
India / IS
Data updates
Latest Update: 2013-12
Total number of updates: 1
Update History
This material has 89 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
IS X04Cr18Ni10 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.08
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
17.00 – 20.00
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 2.00
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
IS 6527: 2006 / Stainless steel wire rod
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
IS X04Cr18Ni10 Physical Properties
Temperature
Modulus of Elasticity
190 — 215
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.61 — 8.1
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 89 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
IS X04Cr18Ni10 Heat Treatments
- Softened: 1000-1120°C, water or air cooled.
- Solution annealed at 1 000 to 1 100°C - If heat treatment is carried out in a continuous furnace, the upper part of the range specified is usually preferred, or even exceeded;
Cooling in water, air - Cooling sufficiently rapidly in order to avoid the occurrence of intergranular corrosion as defined in IS 10461 (Part 2).
IS X04Cr18Ni10 Mechanical Properties
Temperature
Tensile Strength
490 — 700
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
≤ 192
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
≥ 40
%
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 55Cross References
- 21Composition
- 8Mechanical Properties
- 3Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers