11C10S25 (India / IS) Material Properties
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
India / IS
Data updates
Latest Update: 2013-12
Total number of updates: 2
Update History:
2013-11
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.08 – 0.15
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.25
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.35
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2
IS 4431: 1983 / Carbon and carbon manganese free cutting steels
Heat Treatments
- Annealed: 880-930°C; Subcritical annealed: 650-700°C; Carburized: 880-930°C; Refined after carburized: 870-900°C; Hardened after carburized: 760-790°C; Tempered: max. 620°C;
- Carburized: 900-940°C. Direct and single hardened: 830-860°C. Core hardened: 870-890°C. Case hardened: 780-820°C. Quenching media: water, thermal bath at 140-220°C. Tempered: 150-180°C.
-
157 Cross References
-
30 Composition
-
43 Mechanical Properties
-
3 Physical Properties
-
3 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
133 Total Suppliers