IS 25C8 Structural and constructional steels
Data updates
This material has 586 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
IS 25C8 Chemical Composition
IS 1875: 2025 / Steel Ingots, Billets, Blooms, Slabs, and Bars for Forging - Specification
Looking for full material performance data?
Free registration required • Instant access
IS 25C8 Physical Properties
Temperature
This material has 586 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
IS 25C8 Heat Treatments
- Annealed: 870-900°C. Subcritical annealed: 630-700°C. Normalized: 870-900°C. Hardened: 870-900°C. Tempered: max. 660°C.
- Normalized: 880-910°C.
IS 25C8 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
IS 25C8 International Equivalent Materials
Showing 15 of 207 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 207 international equivalents?
See all 207 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 207Cross References
- 79Composition
- 103Mechanical Properties
- 3Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 26Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 164Total Suppliers