PROPRIETARY Uddeholm Hotvar Tool steels
Material group:
Ferrous Alloys / Tool steels
Country / Standard:
PROPRIETARY
Data updates
Latest Update: 2016-11
Total number of updates: 3
Update History
2016-04
2016-01
This material has 42 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Uddeholm Hotvar Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.5500
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
2.6000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.7500
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
Böhler-Uddeholm AG, Product Data Sheets,
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Uddeholm Hotvar Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
Unlock full details
Full data available with free access
View Complete Material Data
Thermal Conductivity
31
W/(m∙°C)
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
This material has 42 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Uddeholm Hotvar Heat Treatments
- Unless otherwise is indicated all specimens were hardened at 1050°C (1920°F), quenched in air and tempered 2+2 h at 575°C (1070°F) to a hardness corresponding to 56 HRC. General recommendations: Soft annealing: Protect the steel and heat through to 820°C (1500°F). Then cool in the furnace at 11°C (20°F) per hour to 600°C (1110°F), then freely in air; Stress relieving: After rough machining the tool should be heated through to 650°C (1200°F), holding time 2 hours. Cool slowly to 350°C (660°F), then freely in air; Hardening: Pre-heating temperature: first step at 480-600°C (895-1110°F), second step at 850 (1560°F). Austenitizing temperature: 1050-1070°C (1920-1960°F), normally 1050°C (1920°F) but when maximum hardness is required the normally temperature is 1070°C (1960°F). (At 1050°C (1920°F) - Soaking time: 30 min, Hardness before tempering for d = 25 mm: 61 ± 1 (Oil) and 59 ±1 (Air); At 1070°C (1960°F) - Soaking time: 20 min, Hardness before tempering for d = 25 mm: 62 ± 1 (Oil) and 60 ±1 (Air)); Quenching media: High speed gas/circulating atmosphere, Vacuum (high speed gas with sufficient positive pressure), Martempering bath or fluidized bed at 450-550°C (840-1020°F), Martempering bath or fluidized bed at approx. 180-220°C (360-430°F), Warm oil, approx. 80°C (175°F). (Temper the tool as soon as its temperature reaches 50-70°C (120-160°F); In order to obtain the optimum properties for the tool, the cooling rate should be fast, but not at a level that gives excessive distortion or cracks.); Tempering: Choose the tempering temperature according to the hardness. Temper minimum twice with intermediate cooling to room temperature. Holding time at temperature minimum 2 h.
PROPRIETARY Uddeholm Hotvar Mechanical Properties
Temperature
Tensile Strength
2100 — 2300
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
210
Unlock full details
Full data available with free access
View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
1800 — 1850
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 6Composition
- 10Mechanical Properties
- 14Physical Properties
- 6Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 2Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 4Total Suppliers