SCMn 5 (Korea / KS) Material Properties

Material group: Ferrous Alloys / Cast steels
Country/Standard: Korea / KS

Data updates

Latest Update: -
Total number of updates: 0
Update History:
-

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 690 MPa view details
Elongation, A 9 % view details
Brinell Hardness (HB) 183 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 100.1 ksi view details
Elongation, A 9 % view details
Brinell Hardness (HB) 183 view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.40 – 0.50
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
1.00 – 1.60
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.040
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

D 4102: 1995 / High Tensile Strength Carbon Steel Castings And Low Alloy Steel Castings For Structural Purposes

Heat Treatments

  • A - Normalizing: 850-950°C; Tempering: 550-650°C B - Quenching: 850-950°C; Tempering: 550-650°C