ASTM A 743 Grade CD-4MCu Cast steels
Data updates
This material has 56 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 743 Grade CD-4MCu Chemical Composition
A743/A743M: 1985 / Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
Looking for full material performance data?
Free registration required • Instant access
ASTM A 743 Grade CD-4MCu Heat Treatments
- Heat to 1040°C (1900°F) minimum, hold for sufficient time to heat casting uniformly to temperature, quench in water or rapid cool by other means to develop acceptable corrosion resistance.
ASTM A 743 Grade CD-4MCu Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 743 Grade CD-4MCu International Equivalent Materials
Showing 15 of 31 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 31 international equivalents?
See all 31 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 31Cross References
- 9Composition
- 3Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 11Total Suppliers