ASTM A 743 Grade CA-40 Cast steels
Data updates
This material has 247 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 743 Grade CA-40 Chemical Composition
A743/A743M: 2021 / Standard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
Looking for full material performance data?
Free registration required • Instant access
ASTM A 743 Grade CA-40 Heat Treatments
- Heat treatment (1): Heat to 955°C (1750°F) minimum, air cool and temper at 595°C (1100°F) minimum, or
Heat treatment (2): Anneal at 790°C (1450°F) minimum.
ASTM A 743 Grade CA-40 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 743 Grade CA-40 International Equivalent Materials
Showing 15 of 129 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 129 international equivalents?
See all 129 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 129Cross References
- 8Composition
- 5Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- 1Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 1Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 101Total Suppliers