ASTM A 271 TP316H Stainless steels

Material group: Ferrous Alloys / Stainless steels
Country / Standard: United States / ASTM

Data updates

Latest Update: -
Total number of updates: 0

This material has 47 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

ASTM A 271 TP316H Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.04 – 0.10
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
16.0 – 18.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 2.00
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

A271: 1985 / Seamless Austenitic Chromium-Nickel Steel Still Tubes for Refinery Service

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

ASTM A 271 TP316H Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 215 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.61 — 8.1 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 47 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

ASTM A 271 TP316H Heat Treatments


  • If cold working is involved in processing, the minimum solution-treating temperature shall be 980°C (1800°F).
    If the material is hot rolled, the minimum solution-treating temperature shall be 980°C (1800°F).

ASTM A 271 TP316H Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≥ 515 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
≤ 192
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
≥ 35 %
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 23Cross References

  • 7Composition
  • 4Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • 3Joints
  • -Coatings
  • 6Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers