ASTM A 426 Grade CP2 Structural and constructional steels
Data updates
This material has 49 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 Grade CP2 Chemical Composition
A426/A426M: 2025 / Standard Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service
Looking for full material performance data?
Free registration required • Instant access
ASTM A 426 Grade CP2 Physical Properties
Temperature
This material has 49 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 Grade CP2 Heat Treatments
- The pipe shall be furnished in the normalized and tempered or liquid-quenched and tempered condition. The temperature for tempering shall not be less than 595°C (1100°F).
ASTM A 426 Grade CP2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 426 Grade CP2 International Equivalent Materials
Showing 9 of 9 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 9 international equivalents?
See all 9 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 9Cross References
- 11Composition
- 5Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 12Creep
- -Joints
- -Coatings
- 8Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers