ASTM A 426 Grade CPCA15 Cast steels
Data updates
This material has 150 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 Grade CPCA15 Chemical Composition
A426/A426M: 2025 / Standard Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service
Looking for full material performance data?
Free registration required • Instant access
This material has 150 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 Grade CPCA15 Heat Treatments
- The pipe shall be furnished in the normalized and tempered or liquid-quenched and tempered condition. The temperature for tempering shall not be less than 675°C (1250°F).
ASTM A 426 Grade CPCA15 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
75 Cross References
-
11 Composition
-
5 Mechanical Properties
-
- Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
8 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
50 Total Suppliers