ASTM A 426 Grade CP12 Structural and constructional steels
Data updates
This material has 139 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 Grade CP12 Chemical Composition
A426/A426M: 2025 / Standard Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service
Looking for full material performance data?
Free registration required • Instant access
ASTM A 426 Grade CP12 Physical Properties
Temperature
This material has 139 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 Grade CP12 Heat Treatments
- The pipe shall be furnished in the normalized and tempered or liquid-quenched and tempered condition. The temperature for tempering shall not be less than 595°C (1100°F).
ASTM A 426 Grade CP12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 426 Grade CP12 International Equivalent Materials
Showing 15 of 48 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 48 international equivalents?
See all 48 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 48Cross References
- 11Composition
- 5Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 12Creep
- 10Joints
- -Coatings
- 8Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 41Total Suppliers