ASTM A 389 Grade C24 Cast steels
Data updates
This material has 105 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 389 Grade C24 Chemical Composition
A389/A389M: 2024 / Standard Specification for Steel Castings, Alloy, Specially Heat Treated, for Pressure Containing Parts, Suitable for High-Temperature Service
Looking for full material performance data?
Free registration required • Instant access
ASTM A 389 Grade C24 Heat Treatments
- Normalizing: 1010 - 1065°C (1850 - 1950°F).
Tempering temperature: 675 - 730°C (1250 - 1350°F), holding time 12h.
Minimum preheat temperature shall be 150°C (300°F).
ASTM A 389 Grade C24 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 389 Grade C24 International Equivalent Materials
Showing 15 of 43 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 43 international equivalents?
See all 43 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 43Cross References
- 8Composition
- 4Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 8Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 41Total Suppliers