AISI 430 Stainless steels
Data updates
This material has 5406 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AISI 430 Chemical Composition
SAE AMS-QQ-S-763D: 2013 / Steel, Corrosion Resistant, Bars, Wire, Shapes and Forgings
Looking for full material performance data?
Free registration required • Instant access
AISI 430 Physical Properties
Temperature
This material has 5406 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AISI 430 Heat Treatments
- As a final heat treatment, tubes shall be reheated to 650°C (1200°F) or higher and cooled.
- Heat treatment shall be performed after welding at minimum 650°C (1200°F), cooling as appropriate for Grade, tempering temperature is not specified.
AISI 430 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AISI 430 International Equivalent Materials
Showing 15 of 339 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 339 international equivalents?
See all 339 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 339Cross References
- 77Composition
- 60Mechanical Properties
- 3Physical Properties
- 5Heat Treatment
- 8Metallography
- 3Machinability
- -Stress-Strain
- 1Formability
- 1Fatigue
- -Fracture
- 28Creep
- 34Joints
- -Coatings
- 83Dimensions
- 12Tribology
- 4502Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 250Total Suppliers