201 (United States / SAE) Material Properties

Material group: Ferrous Alloys / Stainless steels
Country/Standard: United States / SAE

Data updates

Latest Update: 2019-09
Total number of updates: 1
Update History:

Mechanical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 215 GPa view details
Density 7.61 — 8.1 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 31.2 E+03 ksi view details
Density 0.275 — 0.293 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.15
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
16.0 – 18.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
5.5 – 7.5
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
N
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

SAE J 405: 1998 / Chemical compositions of SAE wrought stainless steels

Heat Treatments

  • Annealing: Heating to 1010-1121°C (1850-2050°F). Stress relieving between 468 ± 13.9°C (875 ± 25°F) and 816°C (1500°F) is prohibited. Stress relieving should be at 899°C (1650°F) for 1 hour; water quenching.