AS AS 2074/H5A Cast steels
Data updates
This material has 26 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AS AS 2074/H5A Chemical Composition
AS 2074: 2003 / Cast steels
Looking for full material performance data?
Free registration required • Instant access
AS AS 2074/H5A Heat Treatments
- Grade shall be supplied in the air-quenched or water-quenched condition. The heat treatment shall consist of heating uniformity to an appropriate temperature within the range 1000°C to 1150°C, followed by rapid cooling in air or water.
AS AS 2074/H5A Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AS AS 2074/H5A International Equivalent Materials
Showing 2 of 13 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 13 international equivalents?
See all 13 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 13Cross References
- 7Composition
- 4Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers