SA-540 Grade B24 Class 3 (United States / ASME) Material Properties

Alternative designations: 2Ni-3/4Cr-1/3Mo
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: United States / ASME

Data updates

Latest Update: 2024-02
Total number of updates: 5
Update History:
2024-01 2023-11 2020-05 2016-02

Mechanical Properties


Temperature

≤ 0°C
0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 1000 MPa view details
Tensile Strength val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Elongation, A 12 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Brinell Hardness (HB) 235 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 145 ksi view details
Tensile Strength val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Elongation, A 12 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Brinell Hardness (HB) 235 view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 36.3 W/(m∙°C) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 21 BTU/(h∙ft∙°F) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.37 – 0.44
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.70 – 0.95
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.70 – 0.90
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

ASME Boiler and Pressure Vessel Code An International Code Section II - Part A Ferrous Material Specifications / American Society of Mechanical Engineers / 2023

Heat Treatments

  • Material which is ordered in the annealed condition shall have a structure suitable for machining.<br /> Material which is ordered in the liquid quenched and tempered condition shall be uniformly reheated from a temperature below the cooling transformation range to the proper austenitizing temperature. It shall be quenched in a liquid medium under substanially uniform conditions and then uniformly reheated for tempering. The minimum tempering temperature shall be 455°C (850°F).<br /> Material that has been straightened after quenching and tempering shall be stress relieved by reheating to a temperature not lower than 55°C (100°F) under the tempering temperature.