ASME SA-217 Grade CA15 Cast steels

Alternative designations: 13Cr
Material group: Ferrous Alloys / Cast steels
Country/Standard: United States / ASME

Data updates

Latest Update: 2026-01
Total number of updates: 7
Update History

ASME SA-217 Grade CA15 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.15
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
11.5 – 14.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.00
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

ASME Boiler and Pressure Vessel Code An International Code Section II - Part A Ferrous Material Specifications / American Society of Mechanical Engineers / 2025

Looking for full material performance data?

View Complete Material Data ›

ASME SA-217 Grade CA15 Physical Properties


Temperature

≤ 0°C
0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity val1
Full data available with free access View Complete Material Data
GPa
Unlock full details
Coefficient of Thermal Expansion (CTE) 10.6 10-6/°C Unlock full details
Thermal Conductivity 24.6 W/(m∙°C) Unlock full details

This material has 246 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›

ASME SA-217 Grade CA15 Heat Treatments

  • Furnished in the normalized and tempered condition. Tempered at 595°C (1110°F) minimum.<br />Heat treatment shall be performed after castings have been allowed to cool below the transformation range.<br />Minimum preheat temperature: 200°C (400°F) for all thicknesses.

ASME SA-217 Grade CA15 Mechanical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Yield Strength, Rp0.2 450 MPa Unlock full details
Tensile Strength 620 — 795 MPa Unlock full details
Elongation, A 18 % Unlock full details
Reduction of Area val1
Full data available with free access View Complete Material Data
%
Unlock full details

Mechanical properties are available with full access.

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
  • 41 Cross References

  • 8 Composition
  • 39 Mechanical Properties
  • 78 Physical Properties
  • 1 Heat Treatment
  • - Metallography
  • - Machinability

  • 1 Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • 58 Creep

  • - Joints
  • - Coatings
  • 13 Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 7 Total Suppliers