ASME SA-182 F 429 Stainless steels
Data updates
This material has 180 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASME SA-182 F 429 Chemical Composition
ASME Boiler and Pressure Vessel Code An International Code Section II - Part A Ferrous Material Specifications, American Society of Mechanical Engineers, 2025
Looking for full material performance data?
Free registration required • Instant access
ASME SA-182 F 429 Physical Properties
Temperature
This material has 180 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASME SA-182 F 429 Heat Treatments
- After hot working, forgings shall be cooled to a temperature below 538°C (1000°F) prior to heat treating.
Annealed at min 1010°C (1850°F), furnace cooled.
ASME SA-182 F 429 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASME SA-182 F 429 International Equivalent Materials
Showing 15 of 30 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 30 international equivalents?
See all 30 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 30Cross References
- 7Composition
- 5Mechanical Properties
- 83Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 1Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 49Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 4Total Suppliers