0125 (Sweden / SS) Material Properties
Material group:
Ferrous Alloys / Cast irons
Country/Standard:
Sweden / SS
Data updates
Latest Update: 2025-07
Total number of updates: 1
Update History:
Mechanical Properties
Temperature
Physical Properties
Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.
Register NowComposition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
3.1 – 3.4
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Ceq
VALUE
3.6 – 3.9
UNIT
%
CAS NUMBER
CRITERIA
Mn
VALUE
0.6 – 0.8
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
SS 140125: 1984 / Grey iron - Tensile strength in separately cast and cast-on test samples
Heat Treatments
- For stress relief annealing, a temperature of 550-600°C with a holding time of 1 h is recommended for every 25 mm of material thickness, but at least 1 h. The material should cool slowly (~ 50°C/h) to a temperature below 325°C.
-
1 Cross References
-
6 Composition
-
5 Mechanical Properties
-
- Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
- Total Suppliers