SS 2225-21 Structural and constructional steels
Data updates
This material has 73 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SS 2225-21 Chemical Composition
SS 142225: 1991 / Steel for hardening and tempering - SS-steel 22 25
Looking for full material performance data?
Free registration required • Instant access
SS 2225-21 Physical Properties
Temperature
This material has 73 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SS 2225-21 Heat Treatments
- Normalizing: 840-870°C; Free cooling.
SS 2225-21 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SS 2225-21 International Equivalent Materials
Showing 3 of 60 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 60 international equivalents?
See all 60 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 60Cross References
- 8Composition
- 1Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers