SS 2225-07 Structural and constructional steels
Data updates
This material has 137 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SS 2225-07 Chemical Composition
SS 142225: 1991 / Steel for hardening and tempering - SS-steel 22 25
Looking for full material performance data?
Free registration required • Instant access
SS 2225-07 Physical Properties
Temperature
This material has 137 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SS 2225-07 Heat Treatments
- Tempering: 840-870°C, cooling in oil and 820-850°, cooling in water; The steel should be tempered immediately after cooling. Tempering temperature (550-675°C) and holding time adapted to the dimension and the desired strength; Tempering temperature may go down to 450°C.
SS 2225-07 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SS 2225-07 International Equivalent Materials
Showing 12 of 122 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 122 international equivalents?
See all 122 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 122Cross References
- 7Composition
- 4Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers