STB 35 (Japan / JIS) Material Properties

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Japan / JIS

Data updates

Latest Update: -
Total number of updates: 0
Update History:
-

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 177 MPa view details
Tensile Strength 343 MPa view details
Elongation, A 27 % view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 25.7 ksi view details
Tensile Strength 49.7 ksi view details
Elongation, A 27 % view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.18
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.30 – 0.60
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.035
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

Carbon steel boiler and heat exchanger tubes, JIS G 3461 / 1990

Heat Treatments

  • Hot finished seamless steel tube and hot finished electric resistance welded steel tube: as manufactured, as required, low temperature annealing or normalizing may be performed; Cold finished seamless steel tube: low temperature annealing, normalizing or full annealing; As welded electric resistance welded steel tube and cold finished electric resistance welded steel tube: normalizing.