Mechanical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Yield Strength, Rp0.2 225 MPa view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 400 MPa view details
Elongation, A 18 % view details
Yield Strength, Rp0.2 32.6 ksi view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 58 ksi view details
Elongation, A 18 % view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.25
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
P
VALUE
≤ 0.040
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
≤ 0.040
UNIT
%
CAS NUMBER
7704-34-9

G 3457: 2020 / Arc welded carbon steel pipes

Heat Treatments

  • Pipes shall be either as welded or as cold-expanded after welding and should not normally be subjected to heat treatment.