JIS 46 S 20 Structural and constructional steels
Data updates
This material has 140 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
JIS 46 S 20 Chemical Composition
G 4804: 1999 / Free cutting carbon steels
Looking for full material performance data?
Free registration required • Instant access
JIS 46 S 20 Physical Properties
Temperature
This material has 140 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
JIS 46 S 20 Heat Treatments
- Normalized at 840 to 870°C.
Quenched at 840 to 870°C in oil or water. Time for austenitized as a guide min. 0.5h
Tempered at 540 to 680°C. Time for tempered 1h minimum.
JIS 46 S 20 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
JIS 46 S 20 International Equivalent Materials
Showing 2 of 95 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 95 international equivalents?
See all 95 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 95Cross References
- 6Composition
- 17Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 18Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers