SCS 16A (Japan / JIS) Material Properties

Material group: Ferrous Alloys / Cast steels
Country/Standard: Japan / JIS

Data updates

Latest Update: 2014-11
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 480 MPa view details
Elongation, A 33 % view details
Brinell Hardness (HB) ≤ 183 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 69.6 ksi view details
Elongation, A 33 % view details
Brinell Hardness (HB) ≤ 183 view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.03
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
17.00 – 21.00
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.50
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

G 5121: 2003 / Corrosion-resistant cast steels for general applications

Heat Treatments

  • Solutionizing: 1030-1150°C, rapid cooling.