UNI 16 NiCr 11 Structural and constructional steels
Data updates
This material has 76 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
UNI 16 NiCr 11 Chemical Composition
UNI 8550: 1984 / Special unalloyed and alloyed steel finished products, open die and drop forged, for case hardening. Quality, requirements and tests
Looking for full material performance data?
Free registration required • Instant access
UNI 16 NiCr 11 Physical Properties
Temperature
This material has 76 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
UNI 16 NiCr 11 Heat Treatments
- Hot worked at 1100-900°C; Cementation at 880-900°C; Core hardened at 830-860°C; Surface hardened at 790-820°C. Quenched in hot water bath; Stress relieved at 150-200°C.
UNI 16 NiCr 11 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
UNI 16 NiCr 11 International Equivalent Materials
Showing 8 of 11 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 11 international equivalents?
See all 11 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 11Cross References
- 9Composition
- 18Mechanical Properties
- 17Physical Properties
- 5Heat Treatment
- -Metallography
- -Machinability
- 4Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 12Total Suppliers