AFNOR NF G30Mn6 Cast steels
Material group:
Ferrous Alloys / Cast steels
Country / Standard:
France / AFNOR NF
Data updates
Latest Update: 2018-08
Total number of updates: 2
Update History
2015-09
This material has 114 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
AFNOR NF G30Mn6 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.25 – 0.32
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.80
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
NF A 32-054: 1994 / Foundry products - Cast steels for general purpose in mechanical engineering
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
AFNOR NF G30Mn6 Heat Treatments
- +N: 880-950°C, quenched by air or liquid.
+QT1: 880-950°C, quenched by air or liquid; Tempered at 630-680°C.
+QT2: 880-950°C, quenched by air or liquid; Tempered at 580-630°C. - N: Normalized at 910-970°C, air cooled
QT1: Water or oil quenched, tempered at 580-630°C
QT2: Water or oil quenched, tempered at 630-680°C
AFNOR NF G30Mn6 Mechanical Properties
Temperature
Tensile Strength
520 — 850
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
≥ 10
%
Unlock full details
Full data available with free access
View Complete Material Data
Impact Energy
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
≥ 250
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 44Cross References
- 14Composition
- 54Mechanical Properties
- -Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers