AFNOR NF Z 320 CD 16 3 M Cast irons

Material group: Ferrous Alloys / Cast irons
Country / Standard: France / AFNOR NF

Data updates

Latest Update: 2020-12
Total number of updates: 1
Update History

This material has 20 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

AFNOR NF Z 320 CD 16 3 M Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
2.5 – 3.4
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
14 – 18
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 1.2
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

NF A 32-058: 1984: 1984 / Foundry products - Abrasion resistant cast steels

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

AFNOR NF Z 320 CD 16 3 M Heat Treatments


  • Quenched and tempered (II);
    Air quenched at 900 to 1010°C and tempered at 200 to 300°C. Cooled with an equalization stage at around 500°C in the case of a part sensitive to cracking.
    Structure:
    - for +QT1 condition – Austenitic, martensitic, carbide
    - for +QT2 condition – Martensitic, austenitic, carbide
    Annealed at 680 to 700°C or Full annealed at 950 to 980°C, cooled below 40°C/h up to 600°C

AFNOR NF Z 320 CD 16 3 M Mechanical Properties


Temperature

PROPERTY / VALUE
Brinell Hardness (HB)
350 — 450
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
50 — 64
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

AFNOR NF Z 320 CD 16 3 M International Equivalent Materials


Showing 4 of 4 results.

MATERIAL
STANDARD
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
MATERIAL
STANDARD
DIN
COUNTRY / PRODUCER
Germany
EQUIVALENCE CATEGORY
Official
MATERIAL
STANDARD
B.S.
COUNTRY / PRODUCER
United Kingdom
EQUIVALENCE CATEGORY
Implicit
STANDARD
DIN
COUNTRY / PRODUCER
Germany
EQUIVALENCE CATEGORY
Official
MATERIAL
STANDARD
JUS
COUNTRY / PRODUCER
Yugoslavia
EQUIVALENCE CATEGORY
Implicit

Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.

Need the full list of 4 international equivalents?

See all 4 equivalent grades with detailed mapping by standard, producer and equivalence category.

View All Equivalents ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 4Cross References

  • 9Composition
  • 4Mechanical Properties
  • -Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 2Total Suppliers