AFNOR NF 45 SCD 6 Structural and constructional steels
Data updates
This material has 178 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF 45 SCD 6 Chemical Composition
NF A 35-571 / Iron and steel. Special structural steels suitable for the manufacture of suspension components
Looking for full material performance data?
Free registration required • Instant access
AFNOR NF 45 SCD 6 Physical Properties
Temperature
This material has 178 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF 45 SCD 6 Heat Treatments
- Heated in the range at 865-895°C, cooled in oil and tempered at 550-650°C
Jominy test at 880 ± 5°C. - Annealed: 650-700°C; Oil quenching: 850-880°C; temper: 400-500°C.
AFNOR NF 45 SCD 6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AFNOR NF 45 SCD 6 International Equivalent Materials
Showing 15 of 55 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 55 international equivalents?
See all 55 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 55Cross References
- 28Composition
- 35Mechanical Properties
- 3Physical Properties
- 10Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 46Total Suppliers