DIN 32CrMo12 Structural and constructional steels
Data updates
This material has 303 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 32CrMo12 Chemical Composition
EN 10250-3: 2022 / Open die steel forgings for general engineering purposes - Part 3: Alloy special steels
Looking for full material performance data?
Free registration required • Instant access
DIN 32CrMo12 Physical Properties
Temperature
This material has 303 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 32CrMo12 Heat Treatments
- Hot working: 1100-900°C; Soft annealing: 680-720°C; Normalizing: 880-920°C; Hardening in oil: 860-900°C; Tempering: 540-680°C
- Quenching: 890-940°C, oil, water, or water based solutions; Tempering: 550-740°C.
DIN 32CrMo12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 32CrMo12 International Equivalent Materials
Showing 15 of 143 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 143 international equivalents?
See all 143 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 143Cross References
- 16Composition
- 51Mechanical Properties
- 3Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 86Total Suppliers