12 Ni 19 (Germany / DIN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2020-11
Total number of updates: 1
Update History:
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.15
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr+Cu+Mo
VALUE
≤ 0.50
UNIT
%
CAS NUMBER
CRITERIA
Mn
VALUE
0.30 – 0.80
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2
Flat products made of steels for pressure purposes - Part 4: nickel alloy steels with specified low temperature properties, EN 10028-4 / 1994
Heat Treatments
- Hot working: 1100-850°C; Normalizing: 800-850°C; Tempering: 580-640°C; Hardening (quenching in water or oil): 800-850°C; Tempering: 580-660°C; Stress relieving: 520-560°C
- Hot working: 1100-850°C; Normalizing: 800-850°C; Tempering: 580-640°C; Hardening (quenching in water or oil): 800-850°C; Tempering: 580-660°C; Stress relieving: 520-560°C
-
81 Cross References
-
29 Composition
-
104 Mechanical Properties
-
3 Physical Properties
-
4 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
21 Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
62 Total Suppliers