DIN 21 NiCrMoS 2 Structural and constructional steels
Data updates
This material has 501 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 21 NiCrMoS 2 Chemical Composition
DIN 1652-3: 1990 / Bright steel made from case hardening steel; technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN 21 NiCrMoS 2 Physical Properties
Temperature
This material has 501 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 21 NiCrMoS 2 Heat Treatments
- Carburizing at 880 - 980°C. Core-hardening at 860 - 900°C, case hardening at 780 - 820°C, quenching. Tempering at 150 - 200°C.
DIN 21 NiCrMoS 2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 21 NiCrMoS 2 International Equivalent Materials
Showing 15 of 296 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 296 international equivalents?
See all 296 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 296Cross References
- 16Composition
- 11Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 174Total Suppliers