DIN X 7 NiMo 6 Structural and constructional steels
Data updates
This material has 74 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN X 7 NiMo 6 Chemical Composition
DIN 17280: 1985 / Steels with low temperature toughness; technical delivery conditions for plate, sheet, strip, wide flats, sections, bars and forgings
Looking for full material performance data?
Free registration required • Instant access
DIN X 7 NiMo 6 Physical Properties
Temperature
This material has 74 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN X 7 NiMo 6 Heat Treatments
- H+H+A- Hardening: 850-920°C + 690-740°C; Tempering: 590-630°C Stress relieving: 520-570°C
DIN X 7 NiMo 6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN X 7 NiMo 6 International Equivalent Materials
Showing 1 of 1 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 1 international equivalents?
See all 1 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1Cross References
- 8Composition
- 16Mechanical Properties
- 46Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 2Total Suppliers