DIN 55 Si 7 Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2025-03
Total number of updates: 1
Update History

This material has 260 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 55 Si 7 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.5200 – 0.6000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.7000 – 1.0000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.0500
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

Hot rolled steels for springs suitable for quenching and tempering - Technical delivery conditions, DIN 17221 / 1955

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 55 Si 7 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 260 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 55 Si 7 Heat Treatments

  • Hot forming to forging at 1050-850°C; Hot forming to springs at 900-830°C;
    Annealing at 640-680°C;
    Normalizing at 830-860°C;
    Hardening and tempering: hardening in oil at 830-860°C and tempering at 470-540°C
  • Soft annealing: 650-690°C; Hardening (quenching in oil): 830-860°C; Tempering: 300-500°C

DIN 55 Si 7 Mechanical Properties


Temperature

PROPERTY / VALUE
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Tensile Strength
740 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
6 %
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
235 — 290
Unlock full details
Full data available with free access View Complete Material Data
Vickers Hardness (HV)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 113 Cross References

  • 10 Composition
  • 12 Mechanical Properties
  • 3 Physical Properties
  • 9 Heat Treatment
  • 9 Metallography
  • - Machinability

  • - Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • - Creep

  • 1 Joints
  • - Coatings
  • - Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 103 Total Suppliers