145 Cr 6 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Tool steels
Country/Standard: Germany / DIN

Data updates

Latest Update: -
Total number of updates: 0
Update History:
-

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Brinell Hardness (HB) ≤ 225 view details
Brinell Hardness (HB) ≤ 225 view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.72 — 8 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.279 — 0.289 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.4000 – 1.6000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.3000 – 1.5000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.5000 – 0.7000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

Stahl-Eisen-Liste: Register europäischer Stähle / Verlag Stahleisen GmbH, Düsseldorf / 2003 / 11. Auflage

Heat Treatments

  • Operation of hardening: 820-850°C; Hardness, Brinell, HB 30 < 225; Hardness HRC 64; Hot working 1000-850°C; Soft annealing 780-800°C.