TGL 125 Cr 1 Tool steels
Data updates
This material has 105 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
TGL 125 Cr 1 Chemical Composition
TGL 4393: 1959 / Cold work tool steels; technical specifications for hot rolled bars and steel hammer forgings
Looking for full material performance data?
Free registration required • Instant access
TGL 125 Cr 1 Physical Properties
Temperature
This material has 105 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
TGL 125 Cr 1 Heat Treatments
- Hot forming: 1050-850°C
Soft annealing: 720-750°C
Water hardening: 780-810°C
TGL 125 Cr 1 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
TGL 125 Cr 1 International Equivalent Materials
Showing 2 of 43 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 43 international equivalents?
See all 43 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 43Cross References
- 6Composition
- 4Mechanical Properties
- 3Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 45Total Suppliers