DIN 1.8961 Structural and constructional steels
Data updates
This material has 476 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.8961 Chemical Composition
EN 10025-5: 2019 / Hot rolled products of structural steels - Part 5: Technical delivery conditions for structural steels with improved atmospheric corrosion resistance
Looking for full material performance data?
Free registration required • Instant access
DIN 1.8961 Physical Properties
Temperature
This material has 476 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.8961 Heat Treatments
- Normalized at 890-950°C, cooled in still air
Stress relief annealed at 530-580°C, held for minimum 30 minutes and maximum 150 minutes. For a holding time of more than 90 minutes, it should be aimed for the lower limit of the temperature range
DIN 1.8961 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
116 Cross References
-
29 Composition
-
78 Mechanical Properties
-
3 Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
1 Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
88 Joints
-
- Coatings
-
61 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
99 Total Suppliers