VdTÜV 26 NiCrMo 14 6 Structural and constructional steels
Data updates
This material has 84 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
VdTÜV 26 NiCrMo 14 6 Chemical Composition
WB 390: 1997 / High-strength steel for bolts and nuts, 26 NiCrMo 14 6, material No. 1.6958
Looking for full material performance data?
Free registration required • Instant access
VdTÜV 26 NiCrMo 14 6 Physical Properties
Temperature
This material has 84 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
VdTÜV 26 NiCrMo 14 6 Heat Treatments
- Hardening from hot forming temperature from 840 to 870°C and cooling in water or oil; Tempering from 530 to 620°C or 530 to 580°C, 1h each t <= 50 mm, but not less than 2h, cooling in the air.
VdTÜV 26 NiCrMo 14 6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
VdTÜV 26 NiCrMo 14 6 International Equivalent Materials
Showing 1 of 40 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 40 international equivalents?
See all 40 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 40Cross References
- 10Composition
- 12Mechanical Properties
- 18Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 3Total Suppliers