DIN 1.4959 Chemical Composition
DIN 17459: 1992 / Seamless circular high-temperature austenitic steel tubes; technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN 1.4959 Physical Properties
Temperature
This material has 777 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.4959 Heat Treatments
- Hot working: 1150 - 850°C, air cooling. Annealing: 1100 - 1200°C, water or air cooling.
- Solution heat treatment at 1100 - 1200°C, rapid quenching in water or air. Hot forming at 1150 - 750°C, air quenching.
DIN 1.4959 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.4959 International Equivalent Materials
Showing 15 of 157 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 157 international equivalents?
See all 157 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 157Cross References
- 70Composition
- 137Mechanical Properties
- 109Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- 5Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 1Creep
- 17Joints
- -Coatings
- 136Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 141Total Suppliers