1.3802 (Germany / DIN) Material Properties

Other designations: ,
Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2024-05
Total number of updates: 3
Update History:
2019-04 2014-04

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 590 MPa view details
Elongation, A 25 % view details
Brinell Hardness (HB) ≤ 300 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 85.6 ksi view details
Elongation, A 25 % view details
Brinell Hardness (HB) ≤ 300 view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Density 7.9 kg/dm³ view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 15 W/(m∙°C) view details
Electrical Resistivity 0.8 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Density 0.285 lb/in³ view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 8.67 BTU/(h∙ft∙°F) view details
Electrical Resistivity 481 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.05 – 1.35
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
11 – 14
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.060
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN 10349: 2009 / Steel castings - Austenitic manganese steel castings

Heat Treatments

  • Solution annealed at 1000-1100°C
  • Solution treated at temperature not lower than 1040 °C and quenched in water.